What tubing and MiniPID 2 manifold material do you recommend?

Avoid materials liable to outgas VOCs. Soft plastics contains plasticizer and will emit and adsorb VOCs which will effect measurements. We recommend using fluorinated plastics such as PTFE and PVDF. Please contact sensors@ion.nsrdev.xyz, if you require further support.